雑誌軽金属
Al-0.6%Mg-...

Al-0.6%Mg-1.0%Si合金のベークハード挙動に及ぼす予ひずみ付与および予備時効処理の複合効果

Icons representing 記事

Al-0.6%Mg-1.0%Si合金のベークハード挙動に及ぼす予ひずみ付与および予備時効処理の複合効果

Call No. (NDL)
Z17-284
Bibliographic ID of National Diet Library
10657820
Material type
記事
Author
増田 哲也ほか
Publisher
東京 : 軽金属学会
Publication date
2010-04
Material Format
Paper
Journal name
軽金属 60(4) (通号 594) 2010.4
Publication Page
p.183~189
View All

Holdings of Libraries in Japan

This page shows libraries in Japan other than the National Diet Library that hold the material.

Please contact your local library for information on how to use materials or whether it is possible to request materials from the holding libraries.

other

  • CiNii Research

    Search Service
    Digital
    You can check the holdings of institutions and databases with which CiNii Research is linked at the site of CiNii Research.

Bibliographic Record

You can check the details of this material, its authority (keywords that refer to materials on the same subject, author's name, etc.), etc.

Paper Digital

Material Type
記事
Author/Editor
増田 哲也
高木 康夫
櫻井 健夫 他
Alternative Title
Combined effect of pre-straining and pre-aging on bake-hardening behavior of an Al-0.6mass%Mg-1.0mass%Si alloy
Periodical title
軽金属
No. or year of volume/issue
60(4) (通号 594) 2010.4
Volume
60
Issue
4
Sequential issue number
594