Rodlike capsules consisting of a calcium carbonate core and a crosslinked polystyrene shell were synthesized, and the glass transition temperature (T_...

Search by Bookstore

Holdings of Libraries in Japan

This page shows libraries in Japan other than the National Diet Library that hold the material.

Please contact your local library for information on how to use materials or whether it is possible to request materials from the holding libraries.

other

  • University of Fukui Academic Repository

    Digital
    You can check the holdings of institutions and databases with which Institutional Repositories DataBase(IRDB)(Institutional Repository) is linked at the site of Institutional Repositories DataBase(IRDB)(Institutional Repository).

Bibliographic Record

You can check the details of this material, its authority (keywords that refer to materials on the same subject, author's name, etc.), etc.

Digital

Material Type
文書・図像類
Author/Editor
SASAKI, TAKASHI
MISU, MANABU
SHIMADA, TAKAYUKI
TERAMOTO, MITSUHIRO
Publication, Distribution, etc.
Publication Date
2008-10-01
Publication Date (W3CDTF)
2008-10-01
Periodical title
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS
No. or year of volume/issue
46 19
Volume
46