Chihiro Tabata, Kyoko Kawagishi, Tadaharu Yokokawa, Jun Uzuhashi, Tadakatsu Ohkubo, Hiroshi Harada, Shinsuke SuzukiSpringer Science and Business Media LLC2022-12-24METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE54 5p.1937-1945
インターネットで読める全国の図書館
- 件名Ni-base superalloy oxidation resistance sulfur s...