亀裂を有するセラミッ...

亀裂を有するセラミックスの高温腐食雰囲気中の強度

Icons representing 記事
The cover of this title could differ from library to library. Link to Help Page

亀裂を有するセラミックスの高温腐食雰囲気中の強度

Persistent ID (NDL)
info:ndljp/pid/10479746
Material type
記事
Author
宗像,良幸ほか
Publisher
運輸省船舶技術研究所
Publication date
1995-07-30
Material Format
Digital
Journal name
船舶技術研究所報告 32(1)
Publication Page
p.1-26
View All

Notes on use

Note (General):

著者所属: 船舶技術研究所材料加工部

Detailed bibliographic record

Summary, etc.:

The purpose of this paper is to report on the strengthening mechanism of corroded and/or eroded ceramics at elevated temperature. A study was conducte...

Bibliographic Record

You can check the details of this material, its authority (keywords that refer to materials on the same subject, author's name, etc.), etc.

Digital

Material Type
記事
Author/Editor
宗像,良幸
千田,哲也
Publication, Distribution, etc.
Publication Date
1995-07-30
Publication Date (W3CDTF)
1995-07-30
Alternative Title
Strength of Cracked Ceramics in Hot Corrosive Environments
Periodical title
船舶技術研究所報告
No. or year of volume/issue
32(1)
Volume
32(1)